Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 26.0 g/micron | 660 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 15A Butene HDPE Film Resin Film Properties. Features: Low gel, good barrier properties, strength and toughness.Applications: Lamination, co-extrusion.Data provided by the manufacturer. |
|||
Elmendorf Tear Strength, TD | 26.0 g/micron | 660 g/mil | |
NOVA Chemicals Sclair® FP020-D Octene Copolymer LLDPE Film Resin FP020-D complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FP020.. |
|||
Elmendorf Tear Strength, TD | 26.0 g/micron | 660 g/mil | |
NOVA Chemicals Sclair® FP619-A Octene Copolymer LLDPE Film Resin FP619-A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, withou.. |
|||
Elmendorf Tear Strength, TD | 26.0 g/micron | 660 g/mil | ASTM D1922 |
Chevron Phillips Vytek™ V208A Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Elmendorf Tear Strength, TD | 26.0 g/micron | 660 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 11L1 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion, food and liquid packaging.Data provided by the manufacturer.. |
|||
Elmendorf Tear Strength, TD | 26.0 g/micron @Thickness 0.0250 mm |
660 g/mil @Thickness 0.000984 in |
ASTM D1922 |
Equate EFDA-7047 LLDPE Film Extrusion Resin EFDA-7047 is a linear low-density polyethylene resin for tubular blown film extrusion. Films made from this resin have good toughness, high tensile strength and puncture resistance. EFDA-7047 does n.. |
|||
Elmendorf Tear Strength, TD | 26.0 g/micron | 660 g/mil | ASTM D1922 |
Huntsman Rexell® L8404 Cast Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, and FDA compliant.Applications: Blown film extrusion: general purpose.Film properties based on 1.0 guage (25 µm) thickness; blow-up ratio 2:1.Information provided by H.. |
|||
Elmendorf Tear Strength, TD | 26.0 g/micron | 660 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 11G1 LLDPE Film Resin
(discontinued **) Low gel, Excellent seal characteristics, Easy processabilityApplications: Premium shrink film, Co-extrusionAdditives: Process stabilizer, Polymer process aidFilm properties are typical of blown film.. |
|||
Elmendorf Tear Strength, TD | 26.0 g/micron | 660 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® TF-Y529-BP Hexene LLDPE
(discontinued **) Puncture value is 50 J/mm. Hexene LLDPE. Excellent puncture resistance, good stiffness and machinability, and good tensile properties. Additive Package: High slip and antiblock, process aid.Applic.. |
|||
Elmendorf Tear Strength, TD | 26.0 g/micron | 660 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 11N1 PE Film Resin
(discontinued **) Low gel, Excellent seal characteristics, Easy processabilityApplications: Premium shrink film, Co-extrusionFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are depe.. |
|||
Elmendorf Tear Strength, TD | 26.0 g/micron | 660 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 11C1 Octene LLDPE Film Resin
(discontinued **) Low gel, Good processability, Excellent mechanical propertiesApplications: Shrink filmAdditives: Process stabilizerFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but .. |