Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 8.839 g/micron
224.5 g/mil
ASTM D1922
Dow 650I Low Density Polyethylene Resin
DOW LDPE 650I Resin is intended for use in soft goods over wrap, bread bags, shrink films and other general purpose applications.Information provided by Dow
Elmendorf Tear Strength, TD 8.839 g/micron
224.5 g/mil
ASTM D1922
Dow 611A Low Density Polyethylene (LDPE)
A shrink film resin with good optics packaging applications Optimum gauge range: 1.0 - 3.0 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow