Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 18.7 g/micron | 475 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® HF-Y450-A Hexene HDPE Film Resin Film Properties. Features: High strength and stiffness, excellent drawdown, used in blends with LDPE/LLDPE for improved film stiffness.Applications: Grease barrier, lamination films, blending resin.. |
|||
Elmendorf Tear Strength, TD | 18.7 g/micron | 475 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 19C Homopolymer HDPE Film Resin Film Properties. Features: Good stiffness, good barrier, high clarity, narrow MWD.Applications: Lamination, co-extrusion.Data provided by the manufacturer. |
|||
Elmendorf Tear Strength, TD | 18.7 g/micron | 475 g/mil | ASTM D1922 |
Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4 and LDPE Blend The Trilene® TS 8057 product is a blend with a high ratio of linear low-density polyethylene - butene copolymer (LLDPE) with low-density polyethylene (LDPE) providing elevated processability and en.. |
|||
Elmendorf Tear Strength, TD | 18.7 g/micron | 475 g/mil | ASTM D1922 |
ExxonMobil Exceed™ 399L60 LDPE/Hexene Premium Blown Film Resin, 0.8 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 399L60 resin have balanced tensile, impact strength,.. |
|||
Elmendorf Tear Strength, TD | 18.7 - 26.0 g/micron | 475 - 660 g/mil | Average value: 22.6 g/micron Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Copolymer Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Copolymer Film Grade". Each property range of values reported is minim.. |
|||
Elmendorf Tear Strength, TD | 18.7 g/micron | 474 g/mil | ASTM D1922 |
Huntsman Rexell® M3107 Blown Film Extrusion LLDPE
(discontinued **) Linear-low medium density copolymer, cast film extrusion, FDA compliantFeatures: Excellent combination of stiffness, heat resistance, and impermeability to water vapor.Applications: Food packaging, .. |