Polymer Property : Elmendorf Tear Strength, MD = 264 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 10.4 g/micron
264 g/mil
Dow DOWLEX™ 2045.02 Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2045.02 Polyethylene resin is a premier film resin for general packaging applications ranging from heavy duty applications to high speed, thin gauge applications. It contains high level of ..
Elmendorf Tear Strength, MD 10.4 g/micron
264 g/mil
Dow DOWLEX™ 2045.11 Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2045.11 Polyethylene resin is a premier film resin for general purpose packaging applications, ranging from heavy duty applications to high speed, thin gauge applications. It contains high ..
Elmendorf Tear Strength, MD 10.4 g/micron
264 g/mil
ASTM-D1922
Braskem LL6800N LLDPE Blown Film Extrusion Polyethylene Copolymer
LL6800N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains antiblock, proc..