Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 10.19 g/micron | 258.8 g/mil | ISO 6383-2 |
Polimeri Europa Clearflex® FG 308 Octene Copolymer Linear Low Density Polyethylene Clearflex FG 308 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 308 ar.. |
|||
Elmendorf Tear Strength, MD | 10.19 g/micron | 258.8 g/mil | ISO 6383-2 |
Polimeri Europa Clearflex® FG 368 Octene Comonomer Linear Low Density Polyethylene Clearflex FG 368 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 368 ar.. |
|||
Elmendorf Tear Strength, MD | 10.19 g/micron | 258.8 g/mil | ISO 6383-2 |
Polimeri Europa Clearflex® H&T CLH 150 Linear Low Density Polyethylene Clearflex H&T CLH 150 is a linear low density polyethylene resin, with antioxidants, suitable for cast film extrusion.Stretch films obtained from Clearflex H&T CLH 150 show good optical properties, .. |
|||
Elmendorf Tear Strength, MD | 10.19 g/micron | 258.8 g/mil | ISO 6383/2 |
Borealis FA5223 Low Density Polyethylene FA5223 is a Low Density Polyethylene for Film Extrusion. Contains antioxidant and antiblock additive. This grade is developed to give strong film for medium duty applications. Applications FA5223.. |
|||
Elmendorf Tear Strength, MD | 10.19 g/micron | 258.8 g/mil | ISO 6383/2 |
Borealis FA5224 Low Density Polyethylene FA5224 is a Low Density Polyethylene for Film Extrusion. Contains Antioxidant, Anti-block and Medium Slip additives. This grade is developed to give strong film for medium duty applications. Appl.. |
|||
Elmendorf Tear Strength, MD | 10.19 g/micron | 258.8 g/mil | ISO 6383/2 |
Borealis FT5230 Low Density Polyethylene FT5230 is a Low Density Polyethylene for Film Extrusion. This grade is developed for the production of packaging film with good optical properties for medium duty film applications. Applications: .. |
|||
Elmendorf Tear Strength, MD | 10.19 g/micron | 258.8 g/mil | ISO 6383/2 |
Borealis FT5231 Low Density Polyethylene FT5231 is a Low Density Polyethylene for blown film. Tubular technology. Contains Antioxidant. This grade is developed for the production of packaging film with good optical properties for medium d.. |
|||
Elmendorf Tear Strength, MD | 10.19 g/micron | 258.8 g/mil | ISO 6383/2 |
Borealis FT5232 Low Density Polyethylene FT5232 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes medium slip additive and antioxidant. This grade is developed for the production of packaging film with good op.. |
|||
Elmendorf Tear Strength, MD | 10.19 g/micron | 258.8 g/mil | ISO 6383/2 |
Borealis FT5236 Low Density Polyethylene FT5236 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes anti-block, antioxidant and medium slip additives. Applications FT5236 has been developed especially for applic.. |
|||
Elmendorf Tear Strength, MD | 10.19 g/micron | 258.8 g/mil | ISO 6383/2 |
Borealis Borstar® FB4230 LLDPE for Film Borstar FB4250T is a high molecular weight linear low density polyethylene grade combining good extrusion properties, excellent draw properties and good mechanical strength. Film made from Borstar .. |