Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 3.057 g/micron | 77.65 g/mil | ISO 6383-2 |
Polimeri Europa Clearflex® H&T FHH 508 Octene Copolymer Linear Medium Density Polyethylene Clearflex H&T FHH 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidant, suitable for blown film extrusion.Films obtained from Clearflex H&T FHH 508 show good op.. |
|||
Elmendorf Tear Strength, MD | 3.057 g/micron | 77.65 g/mil | ISO 6383-2 |
Polimeri Europa Riblene® FC 39 Low Density Polyethylene - Blown Film Extrusion Riblene FC 39 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 39 is characterized by a high melt strength leading to a good bubble stability.. |
|||
Elmendorf Tear Strength, MD | 3.057 g/micron | 77.65 g/mil | ISO 6383-2 |
Polimeri Europa Riblene® FF 22 Low Density Polyethylene - Blown Film Extrusion Riblene FF 22 is a high molecular weight low density polyethylene (LDPE), with added slip agent, suitable for blown film extrusion. Riblene FF 22 is characterized by a good melt strength leading to.. |
|||
Elmendorf Tear Strength, MD | 3.057 g/micron | 77.65 g/mil | ISO 6383-2 |
Polimeri Europa Greenflex® FD 53 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 53 is an ethylene vinyl acetate copolymer (EVA), containing antiblocking agent, for blown film extrusion. Films produced with Greenflex FD 53 exhibit good sealing properties, high flex.. |