Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 12.1 MPa
1750 psi
at 2% offset; ASTM D882
ExxonMobil LL 3105.50 Premium High Strength Film Resin  (discontinued **)
LL 3150.32 is a hexene copolymer LLDPE film resin for blown film. Films produced from this resin have excellent tensile and toughness properties, as well as improved stiffness. Combined with good dr..
Film Tensile Strength at Yield, TD 12.1 - 228 MPa
1750 - 33000 psi
Average value: 31.5 MPa Grade Count:71
Overview of materials for High Density Polyethylene (HDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max..
Film Tensile Strength at Yield, TD 12.1 MPa
1750 psi
at 2% offset; ASTM D882
ExxonMobil Pax-Plus™ 3201 Blown Film Resin
Pax-Plus 3201 is a rubber modified high density polyethylene film resin that exhibits excellent impact strength and stress crack resistance. It is used primarily in film where its good tear resista..
Film Tensile Strength at Yield, TD 12.1 MPa
1750 psi
Dow DOWLEX™ 2045.02 Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2045.02 Polyethylene resin is a premier film resin for general packaging applications ranging from heavy duty applications to high speed, thin gauge applications. It contains high level of ..
Film Tensile Strength at Yield, TD 12.1 MPa
1750 psi
Dow DOWLEX™ 2045.11 Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2045.11 Polyethylene resin is a premier film resin for general purpose packaging applications, ranging from heavy duty applications to high speed, thin gauge applications. It contains high ..
Film Tensile Strength at Yield, TD 12.1 MPa
1750 psi
Dow LDPE 609A Low Density Polyethylene, High Clarity Film Grade
DOW LDPE 609A resin is a fully formulated high strength clarity film resin for optical packaging applications, such as produce and bakery film. It contains medium levels of slip additive and low lev..