Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 89.6 MPa | 13000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 054 Polyester Film Melinex® 054 is a high clarity, low balanced shrink polyester film which is two-side pretreated to promote adhesion to industrial coatings and inks.Information provided by DuPont. |
|||
Film Tensile Strength at Yield, TD | 89.6 MPa | 13000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 301H Polyester Film Melinex® 301H is a coextruded film that is one side heat sealable and is able to accept many industrial coatings.Information provided by DuPont. |
|||
Film Tensile Strength at Yield, TD | >= 89.6 MPa | >= 13000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 461 Polyester Film Melinex® 461 is a high clarity polyester film manufactured with a coating on one surface that promotes adhesion to many solvent formulations and to most vinyl or acrylic base ink systems. The adhes.. |
|||
Film Tensile Strength at Yield, TD | >= 89.6 MPa | >= 13000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 473 Polyester Film, 200 Gauge Melinex® 473 is a high clarity polyester film manufactured with a coating on one surface that improves slip and handling characteristics. The opposite surface is raw polyester (non-coated). The sli.. |
|||
Film Tensile Strength at Yield, TD | >= 89.6 MPa | >= 13000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 478 Polyester Film, 200 Gauge Melinex® 478 is a high clarity polyester film manufactured with a coating on both surfaces that improves slip and handling characteristicsTypical Applications: Melinex 478 is used in many general i.. |
|||
Film Tensile Strength at Yield, TD | 89.6 MPa | 13000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 725 Polyester Film Melinex® 725 is a high clarity polyester film pretreated on both sides to promote adhesion to many industrial coatings and inks. Melinex® 725 exhibits improved performance in multi-pass printing a.. |
|||
Film Tensile Strength at Yield, TD | 89.6 MPa | 13000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 523 Polyester Film Melinex® 523 is a high clarity polyester film. It is pretreated on both surfaces with MAP (multiple application pretreatment) to promote adhesion to most aqueous and solvent coating formulations. I.. |