Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD >= 24.0 MPa
>= 3480 psi
ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4118Q (18403) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Film Tensile Strength at Yield, TD 24.0 MPa
3480 psi
ASTM D882
NOVA Chemicals Novapol® HF-Y450-A Hexene HDPE Film Resin
Film Properties. Features: High strength and stiffness, excellent drawdown, used in blends with LDPE/LLDPE for improved film stiffness.Applications: Grease barrier, lamination films, blending resin..
Film Tensile Strength at Yield, TD >= 24.0 MPa
>= 3480 psi
ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4117P (18402) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Film Tensile Strength at Yield, TD >= 24.0 MPa
>= 3480 psi
ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4118P (18402) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Film Tensile Strength at Yield, TD 24.0 MPa
3480 psi
ISO 527-3
Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film
Lumicene® mPE M 6040 S01 is a second generation metallocene high density polyethylene.Lumicene® mPE M 6040 S01 can be processed at high output rates with low extrusion pressure, low neck-in, excel..
Film Tensile Strength at Yield, TD 24.0 MPa
3480 psi
ISO 527-3
Dow INSPIRE™ 112 Performance Polymer
INSPIRE™ 112 Performance Polymer is a propylene-based resin intended for use in film and sheet extrusion.Information provided by Dow
Film Tensile Strength at Yield, TD 24.0 MPa
3480 psi
ASTM D882
Braskem HF 0144 HDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras..