Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 36.0 GPa | 5220 ksi | calculated |
Schott N-BAF51 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 36.0 GPa | 5220 ksi | calculated |
Schott N-SF1 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 36.0 GPa | 5220 ksi | calculated |
Schott N-SF15 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 36.0 GPa | 5220 ksi | calculated |
Schott N-SF4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 36.0 GPa | 5220 ksi | calculated |
Schott P-SF67 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 36.0 GPa | 5220 ksi | calculated |
Schott N-LAF2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 36.0 GPa | 5220 ksi | calculated |
Schott N-LAK21 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 36.0 GPa | 5220 ksi | calculated |
Schott N-LAK22 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 36.0 GPa | 5220 ksi | Calculated |
Advanced Ceramics ZEMAT® ACL 2090 - Zero Expansion Glass-Ceramic “Zero Expansion” glass-ceramic is a transparent material now in production for applications requiring ultra-low thermal expansion. The primary crystal phase is a s-eucryptite (Li2OAl2O32SiO2) soli.. |
|||
Shear Modulus | 36.0 GPa | 5220 ksi | calculated |
Schott N-KZFS5 Glass Information Provided by SCHOTT North America, Inc. |