Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.400 - 0.500 GPa | 58.0 - 72.5 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Hyflon® MFA® F1520 Perfluoropolymer Hyflon® F is a family of MFA polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistance, low s.. |
|||
Tensile Modulus | 0.400 - 0.500 GPa | 58.0 - 72.5 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Hyflon® MFA® F1530 Perfluoropolymer Hyflon® MFA is a family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistanc.. |
|||
Tensile Modulus | 0.400 - 0.500 GPa | 58.0 - 72.5 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Hyflon® MFA® F1540 Perfluoropolymer Hyflon® MFA is a unique family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame re.. |
|||
Tensile Modulus | 0.400 - 0.500 GPa | 58.0 - 72.5 ksi | MD/TD; ISO 527-3 |
Borealis BorPure™ RD226CF Polypropylene Random Copolymer BorPure™ RD226CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: BorPure™ RD226CF is recommended for food packaging.. |
|||
Tensile Modulus | 0.400 - 0.500 GPa | 58.0 - 72.5 ksi | MD/TD; ISO 527-3 |
Borealis BorPURE™ RD266CF Polypropylene Random Copolymer BorPure™ RD266CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: BorPure™ RD266CF is recommended for
food packaging.. |
|||
Tensile Modulus | 0.400 - 0.500 GPa | 58.0 - 72.5 ksi | MD/TD; ISO 527-3 |
Borealis BorPURE™ RE216CF Polypropylene Random Copolymer BorPure™ RE216CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films for metallization. Applications: BorPure™ RE216CF is recommended for Lamination films, Me.. |
|||
Tensile Modulus | 0.400 - 0.500 GPa | 58.0 - 72.5 ksi | MD/TD; ISO 527-3 |
Borealis RD735CF Polypropylene Random Copolymer RD735CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD735CF is recommended for food packaging, textile packaging .. |