Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0600 GPa | 8.70 ksi | 1 mm/min; ASTM D638 - ISO 527-2 |
DuPont Elvaloy® 1214 AC Ethylene and 14% Methyl Acrylate Copolymer
(discontinued **) Elvaloy® 1214 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Tensile Modulus | 0.0600 GPa | 8.70 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON TX06488NTX1 PU LNP* STAT-KON* TX06488NTX1 is a compound based on Polyurethane resin containing Proprietary Filler(s). Added features of this grade are: Execllent Ductility, Electrically Conductive. |
|||
Tensile Modulus | 0.0600 GPa | 8.70 ksi | ISO 527-1/-2 |
DSM Arnitel® PL380 38 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.0600 GPa | 8.70 ksi | ISO 527-1/-2 |
DSM Arnitel® PL380 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.0600 GPa | 8.70 ksi | ISO 527-1/-2 |
DSM Arnitel® PL381 Injection Molding Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.0600 GPa | 8.70 ksi | ISO 527-1/-2 |
DSM Arnitel® PL381 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.0600 GPa | 8.70 ksi | ISO 527-1/-2 |
DSM Arnitel® PL381-H TPC-ET Injection Molding |
|||
Tensile Modulus | 0.0600 GPa | 8.70 ksi | ISO 527-1/-2 |
DSM Arnitel® PM381 38 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.0600 GPa | 8.70 ksi | ISO 527-1/-2 |
DSM Arnitel® PM381 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.0600 GPa | 8.70 ksi | ISO 527-1/-2 |
DSM Arnitel® VT3104 TPC-ET Extrusion Grade |
|||
Tensile Modulus | 0.0600 GPa | 8.70 ksi | ISO 527-1/-2 |
DSM Arnitel® XG5857 TPC-ET Extrusion Grade |
|||
Tensile Modulus | 0.0600 GPa | 8.70 ksi | average; in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® C71.75 Elevated Temperature Structural Foam AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength.. |