Mechanical Properties Metric English Comments
Tensile Modulus 5.05 GPa
732 ksi
ISO 527-1/2
Radici Radilon® ACP300 K (dry) Nylon 66
Heat stabilized mineral filledInformation provided by Radici group.
Tensile Modulus 5.05 GPa
732 ksi
ISO 527-1/2
Radici Radilon® AERV1906 LK (dry) Nylon 66
Glass-fiber reinforced with high impact strength, heat stabilizedInformation provided by Radici group.
Tensile Modulus 5.05 GPa
732 ksi
Radici Radilon® S CP300 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.