Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.21 GPa | 611 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp DFI12E PC (Asia Pacific) LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli.. |
|||
Tensile Modulus | 4.21 GPa | 611 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp DFI12E PC LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli.. |
|||
Tensile Modulus | 4.21 GPa | 611 ksi | ASTM D638 |
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon PAI grades cannot be molded successfully in molds with undercuts. Torlon 4601 has been formulated to be moldable.. |
|||
Tensile Modulus | 4.21 GPa | 611 ksi | ASTM D638 |
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI) Torlon® 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon® PAI grades cannot be molded successfully in molds with undercuts. Torlon® 4601 has been formulated to.. |
|||
Tensile Modulus | 4.21 GPa | 611 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp FF004 PE LNP THERMOCOMP* FF004 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 4.21 GPa | 611 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp KB004 Acetal Copolymer LNP THERMOCOMP* KB004 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 4.21 GPa | 611 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East) 6.5% glass reinforced, Super High Flow, flame retardant PBT. |