Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D822 |
DuPont Teijin Films Mylar® A Polyester Film, 1000 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D822 |
DuPont Teijin Films Mylar® A Polyester Film, 1200 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D822 |
DuPont Teijin Films Mylar® A Polyester Film, 1400 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D822 |
DuPont Teijin Films Mylar® A Polyester Film, 142 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D822 |
DuPont Teijin Films Mylar® A Polyester Film, 200 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D822 |
DuPont Teijin Films Mylar® A Polyester Film, 75 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D882 |
DuPont Teijin Films Mylar® MDA Polyester Film, 1000 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D882 |
DuPont Teijin Films Mylar® MDA Polyester Film, 1200 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D882 |
DuPont Teijin Films Mylar® MDA Polyester Film, 1400 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D882 |
DuPont Teijin Films Mylar® MDA Polyester Film, 75 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D882 |
DuPont Teijin Films Mylar® MDA Polyester Film, 750 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D882A |
DuPont Teijin Films Mylar® TL Polyester Film Mylar® Type TL film is a film specified for card protection engineered to provide an identical shrinkage between MD/TD and also possessing good properties of resistance to moisture, oils and chemic.. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D822 |
DuPont Teijin Films Mylar® A Polyester Film, 300 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D822 |
DuPont Teijin Films Mylar® A Polyester Film, 400 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D822 |
DuPont Teijin Films Mylar® A Polyester Film, 48 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D822 |
DuPont Teijin Films Mylar® A Polyester Film, 500 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D822 |
DuPont Teijin Films Mylar® A Polyester Film, 750 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D822 |
DuPont Teijin Films Mylar® A Polyester Film, 900 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D822 |
DuPont Teijin Films Mylar® A Polyester Film, 92 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D882 |
DuPont Teijin Films Mylar® MDA Polyester Film, 142 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D882 |
DuPont Teijin Films Mylar® MDA Polyester Film, 300 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D882 |
DuPont Teijin Films Mylar® MDA Polyester Film, 400 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D882 |
DuPont Teijin Films Mylar® MDA Polyester Film, 48 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D882 |
DuPont Teijin Films Mylar® MDA Polyester Film, 500 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D882 |
DuPont Teijin Films Mylar® MDA Polyester Film, 900 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D882 |
DuPont Teijin Films Mylar® MDA Polyester Film, 92 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D-638 |
Axiall 7777 Rigid PVC, Extrusion Georgia Gulf 7777 is a rigid PVC compound designed for outdoor applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D882 |
DuPont Teijin Films Mylar® MDA Polyester Film, 200 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |