Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.45 GPa | 500 ksi | MD, supporting material; ASTM D882 |
Rogers Corporation Poron® 4701-30-20 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which ena.. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | MD, supporting material; ASTM D882 |
Rogers Corporation Poron® 4790-92-12 P Series Urethane Foam, Extra Soft, Slow Rebound, PET Film Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | MD, supporting material; ASTM D882 |
Rogers Corporation Poron® 4790-92-30012 P Urethane Foam, Extra Soft, Slow Rebound, PET Film Reinforced Extra soft, slow rebound with a very low closure force. Available with thickness of 0.012" (0.30 mm).Features and Benefits of PORON Products: Excellent compression set resistance which enables dura.. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | MD, supporting material; ASTM D882 |
Rogers Corporation Poron® Shock Seal™ 4790-79-12 Handheld Urethane Foam, Handheld Grade, PET Reinforced Extreme Impact Protection, Ultimate ReliabilitySpecifically engineered to protect sensitive components from damage caused by impactConsistent cushioning performance through repeated impactsExcellent.. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | MD, supporting material; ASTM D882 |
Rogers Corporation Poron® 4701-30-25 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which enab.. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | Dried; ISO 527 |
Manifattura Cattaneo PA 6.6 Nylon Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | ISO 527 |
Manifattura Cattaneo PET+PTFE Polyethylene Terephthalate Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | |
Master Bond EP45HTQ Quartz Filled Heat Resistant Epoxy Description: Master Bond Polymer Compound EP45HTQ is a two component quartz filled, epoxy compound for high performance structural bonding and casting. It is suitable for applications where long ter.. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | ASTM D638 |
Ensinger Tecapeek® XP-119 Compression Molded PEEK Compound, 10% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ MP-10GF/10T Modified Polyphenylene Oxide (mPPO), Glass Filled, PTFE Lubricated
(discontin Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 HB (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® UR-20CF/000 Thermoplastic Elastomer - TPU, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | ASTM D638 |
PolyOne Edgetek® UR-20GF/000 Natural Thermoplastic Polyurethane (Ether-Based), 20% Glass Fiber Reinforced
(di Information provided by PolyOne™ Corporation |