Polymer Property : Tensile Modulus = 425 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.93 GPa
425 ksi
ASTM D638
Quadrant EPP Quadrant Nylon 101 Extruded, Unfilled, Type 66 Natural and Black (ASTM Product Data Sheet)
Tensile Modulus 2.93 GPa
425 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP COLORCOMP JX91550 PES
LNP COLORCOMP* JX91550 is an unfilled Polyethersulfone.
Tensile Modulus 2.93 GPa
425 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP COLORCOMP JX91550 PES (Asia Pacific)
LNP COLORCOMP* JX91550 is a compound based on Polyethersulfone resin containing Unfilled Custom Color.
Tensile Modulus 2.93 GPa
425 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycolac® BDT5510 ABS
Automotive. High heat resistance, low gloss, color concentratable for interior applications. Natural only.
Tensile Modulus 2.93 GPa
425 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Fittings M1012 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Modulus 2.93 GPa
425 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RI001 PA 66
LNP* LUBRICOMP* RI001 is a compound based on Nylon 66 resin containing 2% Silicone. Added feature of this grade is: Wear Resistant.
Tensile Modulus 2.93 GPa
425 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Noryl PX0346 PPE+PS
This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 2.93 GPa
425 ksi
ASTM D638
Ensinger HYDEX® 4101 Polybutylene Terephthalate (PBT)
HYDEX® 4101 & 4101L (lubricated) is a very stable chemical compound that can withstand high impact without deterioration. It is approved for direct contact with food by the FDA and is ideal for ma..