Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.45 GPa | 356 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® HG-0760LT ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.45 GPa | 356 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® BF-0679P MABS, Unreinforced Scratch Resistant Scratch resistant material that is used for the exterior material of flat TVInformation provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.45 GPa | 356 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® HG-0760LT ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.45 GPa | 356 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® BF-0679P MABS, Unreinforced Scratch Resistant Scratch resistant material that is used for the exterior material of flat TVInformation provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.46 GPa | 356 ksi | Storage |
Epoxy Technology EPO-TEK® 354 High Temperature Epoxy Product Description: EPO-TEK® 354 is a two component, high Tg epoxy designed for semiconductor packaging in medical, fiber optic and optoelectronic assemblies. It is an electrically and thermally i.. |
|||
Tensile Modulus | 2.45 GPa | 356 ksi | ASTM D-638 |
Axiall 8132 Rigid PVC, Extrusion Georgia Gulf 8132 is a rigid PVC compound designed for applications where transparency is important. This product remains unchanged except for the coded name and was previously identified as 3132. .. |