Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Spartech 513 Static Dissipative Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Spartech 617 Static Dissipative Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Spartech Noryl® SP-5210 Specialty Sheet Description: Specialty SheetNoryl is a registered trademark of General Electric Company.Information provided by Spartech. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D882 |
Spartech PETG 3D Lenticular 3-D Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Star Plastics ABS405 Extrusion Grade ABS Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Styron Pulse® 2100LG ABS + PC Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Westlake Plastics Absylux® FR Acrylonitrile-Butadiene-Styrene Flame Retardant Absylux ABS is a low cost engineering plastic that is easy to machine and fabricate. It is an ideal material for structural applications when impact resistance, strength, and stiffness are required.. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | 50 mm/min; ASTM D638 |
Dow CALIBRE™ MEGARAD™ 2081-15 Polycarbonate CALIBRE™ MEGARAD™ 2081-15 resin is specially formulated to meet the radiation sterilization needs of the healthcare industry, while providing exceptional clarity, heat resistance, impact strength.. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Ensinger DELRIN® AF DE588 Acetal Homopolymer, 20% PTFE filled (POM) DELRIN® AF DE588 is a 20% PTFE filled homopolymer acetal that is fully tested and certified for use by the United States Navy. The resin is manufactured by DuPont and is used extensively in a varie.. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Amco Amalloy® B9336 Polymer Alloy Amco Amalloy B9336 is a clear performance copolymer with exceptional clarity and toughness.Stiff, with good tensile and flexural strength.Information provided by Amco Plastic Materials. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D-638 |
Axiall 8302 Rigid PVC, Extrusion & Molding Georgia Gulf 8302 is a clear rigid PVC pellet compound suited for applications where transparency is important in a high sunlight environment. It can be used for exterior transparent profiles such .. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Quadrant EPP Quadrant LSG PC (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | TM R050-36 |
Resinlab® EP1199 Black Unfilled Epoxy Adhesive Resinlab™ EP1199 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and.. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Spartech Spectar® UV Copolyester Sheet Description: Copolyester SheetSpectar is a registered trademark of Eastman Chemical Company.Information provided by Spartech. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | TM R050-36 |
Resinlab® EP1199 Clear Unfilled Epoxy Adhesive Resinlab™ EP1199 Clear is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and.. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D-638 |
Axiall SP-6235 Rigid PVC, Molding Georgia Gulf SP-6235 is a high flow rigid PVC compound designed for electrical and custom molding applications. This compound features excellent physical properties, high melt flow and exceptionall.. |