Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.200 GPa | 29.0 ksi | 1mm/min; DIN 53457 |
Advanced Elastomer Systems VistaFlex® 911-B Thermoplastic Rubber
(discontinued **) Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f.. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | |
LyondellBasell Lupolen® 2012 D SW 413 LDPE Cable sheathingData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | |
LyondellBasell Lupolen® 2210 H SK LDPE Cable sheathingData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | ISO 527 |
FKuR Kunststoff Terralene® LL 1303 Biobased Polyethylene With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol.. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | 1 mm/min; ASTM D638 |
ICO Polymers ICOFLOâ„¢ 510-5018 400 Micron LDPE Powder Description: ICOFLO 510-5018 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | 1 mm/min; ASTM D638 |
ICO Polymers ICOFLOâ„¢ 510-5054 800 Micron LDPE Powder Description: ICOFLO 510-5054 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | |
LyondellBasell Lupolen® 1842 D SW 413 LDPE Cable sheathingData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | |
LyondellBasell Lupolen® 2003 H LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | |
LyondellBasell Lupolen® 1800 S LDPE, Injection Molding Grade Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | |
LyondellBasell Lupolen® 1810 D LDPE Blow moldings, sheet, profile, film.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | |
LyondellBasell Lupolen® 1810 E LDPE Blow moldingData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | |
LyondellBasell Lupolen® 1810 H LDPE, Injection Molding Grade Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | |
LyondellBasell Lupolen® 1812 D LDPE Insulation for cableData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | |
LyondellBasell Lupolen® 1812 E LDPE Insulation for cableData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | |
LyondellBasell Lupolen® 1840 H LDPE Blow moldings, injection moldings, film.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP PDXF89080 PE LNP* LUBRICOMP* PDXF89080 is a compound based on Polyethylene containing Proprietary Fillers. Added feature of this grade is: Wear Resistant. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp YP003 TPEE LNP LUBRICOMP* YP003 is a compound based on TPEE resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas .. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | MD; ASTM D882-A |
Borealis FA6220 Low Density Polyethylene FA6220 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant. This grade is developed for the production of thin blown films. Applications: shrink film, pouches, general packagin.. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | MD; ASTM D882-A |
Borealis FA6224 Low Density Polyethylene FA6224 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Contains Antioxidant, Anti-block and Medium Slip additives. This grade is developed for the production of thin blown f.. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | MD; ASTM D882-A |
Borealis FA7220 Low Density Polyethylene FA7220 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant. This grade is developed for production of blown film or cast film with good optical properties. When cast on a polish.. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | MD; ASTM D882-A |
Borealis FA7224 Low Density Polyethylene FA7224 has been developed for applications such as: Thin bags with excellent optical and slip properties, and laundry and other textile bags. Contains antioxidant.Information provided by Borealis AG.. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | MD; ASTM D882-A |
Borealis FA7229 Low Density Polyethylene FA7229 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant and Cling additive. Applications: food wrap film, lamination films, blending, and other blown cling film.Information pr.. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | ISO 527-1/-2 |
DSM Arnitel® EM550 55 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | ISO 527-1/-2 |
DSM Arnitel® PM460 General Purpose Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | ISO 527-1/-2 |
DSM Arnitel® PM460 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | ISO 527-2/1A/1 |
ExxonMobil LDPE LD 653 Low Density Polyethylene Resin (European Grade) Product Description: LD 653 is an easy flowing LDPE grade with medium stiffness and good toughness.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: .. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | ISO 527-1/-2 |
DSM Arnitel® EL550 55 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | ISO 527-1/-2 |
DSM Arnitel® EL550 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | ISO 527-1/-2 |
DSM Arnitel® UM551 55 Shore D Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.200 GPa | 29.0 ksi | |
LyondellBasell Lupolen® 1800 H LDPE, Injection Molding Grade Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |