Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 19.7 GPa | 2860 ksi | 5.0 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical prope.. |
|||
Tensile Modulus | 19.7 GPa @Temperature 23.0 °C |
2860 ksi @Temperature 73.4 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention.. |
|||
Tensile Modulus | 19.7 GPa | 2860 ksi | 5 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber KetaSpire® KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanic.. |
|||
Tensile Modulus | 19.7 GPa @Temperature 23.0 °C |
2860 ksi @Temperature 73.4 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of .. |