Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 17.9 GPa @Temperature 23.9 °C |
2600 ksi @Temperature 75.0 °F |
Dry; ASTM D638 |
Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.Key Features and Benefits:Self adhesive resin system f.. |
|||
Tensile Modulus | 17.9 GPa | 2600 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PK-30CF/000 Polyetheretherketone (PEEK), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 17.9 GPa | 2600 ksi | 5 mm/min; ASTM D638 |
LNP ULTEM® EXCP0096 Polyetherimide, 30% Carbon Fiber Reinforcement, 10% PTFE Lubricant
(discontinued **) Features: Lubricated, Electrically Conductive, Good Wear Resistance, High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This dat.. |
|||
Tensile Modulus | 17.9 GPa | 2600 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Therma-Tech™ LC-5000C TC LCP
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Tensile Modulus | 17.9 GPa | 2600 ksi | ASTM D638 |
Quantum Composites QC-7752 50% Glass Fiber Heat Resistant Polyester SMC
(discontinued **) QC-7752 is a modified polyester sheet molding compound (SMC) that is designed for applications requiring high strength, good environmental resistance, and resistance to elevated temperatures. It of.. |
|||
Tensile Modulus | 17.9 GPa | 2600 ksi | |
MTI ThermoStran® PA66-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Tensile Modulus | 17.9 GPa | 2600 ksi | ISO 527-2 |
Solvay Specialty Polymers Kalix® 3850 Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 3850 is a 16% bio-sourced, amorphous polyphthalamide (PPA)-based compound with 50% by weight glass fiber reinforcement. This material is uniquely formulated to prevent warpage and flash in.. |
|||
Tensile Modulus | 17.9 GPa | 2600 ksi | ASTM D638 |
Solvay Specialty Polymers Xydar® MG-850 Liquid Crystal Polymer (LCP), 50% GlassMineral Xydar® MG-850 liquid crystal polymer (LCP) is a 50% glass/mineral reinforced injection molding grade developed for electrical/electronic applications utilizing surface mount technology. The mater.. |
|||
Tensile Modulus | 17.9 GPa | 2600 ksi | ASTM D638 |
Sumitomo Bakelite Sumikon® PM-9501 Glass-Filled Phenolic, Injection Grade Sumikon PM-9501 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s.. |
|||
Tensile Modulus | 17.9 GPa | 2600 ksi | ASTM D638 |
Ensinger Tecapeek® XP-111 Compression Molded PEEK Compound, 50% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |