Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 15.6 GPa | 2260 ksi | ASTM D638 |
Parker Chomerics PREMIER™ A240-ST EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Tensile Modulus | 15.58 GPa | 2260 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP EX93452 PEI (Asia Pacific) LNP* THERMOCOMP* EX93452 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 15.6 GPa | 2260 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON RE0039 PA 66 LNP STAT-KON* RE0039 is a compound based on Nylon 66 resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Tensile Modulus | 15.6 GPa | 2260 ksi | ASTM D638 |
Plenco 6343 Phenolic, Granular, Compression Molded PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz.. |
|||
Tensile Modulus | 15.6 GPa | 2260 ksi | ISO 527-1/-2 |
DSM Arnite® TV4 290 PBT-GF50 50% Glass Reinforced |
|||
Tensile Modulus | 15.6 GPa | 2260 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® DW-1150 Polyphthalamide (PPA)
(Unverified Data**) Amodel DW-1150 is a 50% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of th.. |