Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 2012 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 13.87 GPa
2012 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON MV00AS PP (Asia Pacific)
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Tensile Modulus 13.87 GPa
2012 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Verton MX03017 PP (Europe-Africa-Middle East)
LNP* VERTON* MX03017 is a compound based on Polypropylene resin containing Glass Fiber, Long Glass Fiber. Added features of this material include: Chemically Coupled.This data was supplied by SABIC..
Tensile Modulus 13.87 GPa
2012 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON REF42I PA 66
LNP* STAT-KON* REF42I is a compound based on Nylon 6/6 containing Proprietary Fillers. Added feature of this grade is: Electrically Conductive.
Tensile Modulus 13.87 GPa
2012 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON MV00ASXP PP (Europe-Africa-Middle East)
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Tensile Modulus 13.87 GPa
2012 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON MV00AS PP
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing 50% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, Structural.
Tensile Modulus 13.87 GPa
2012 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON MV00ASU PP
LNP VERTON* MV00ASU is a compound based on Polypropylene resin containing 50% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur..
Tensile Modulus 13.87 GPa
2012 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON MV00ASU PP (Asia Pacific)
LNP VERTON* MV00ASU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Tensile Modulus 13.87 GPa
2012 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON MV00ASU PP (Europe-Africa-Middle East)
LNP VERTON* MV00ASU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.