Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.44 GPa | 1804 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP UF006H PPA LNP* THERMOCOMP* UF006H is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Tensile Modulus | 12.44 GPa | 1804 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP UF006H PPA (Asia Pacific) LNP* Thermocomp* UF006H is a compound based on Polyphthalamide resin containing Glass Fiber. |