Polymer Property : Tensile Modulus = 1485 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 10.24 GPa
1485 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP KFL25 Acetal Copolymer
LNP LUBRICOMP* KFL25 is a compound based on Acetal Copolymer resin containing 25% Glass Fiber, 10% PTFE. Added feature of this material is: Wear Resistant.
Tensile Modulus 10.24 GPa
1485 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP QFN16 PA 6/10
LNP* LUBRICOMP* QFN16 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 5% MOS2. Added feature of this material is: Wear Resistant.