Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.00 GPa | 1020 ksi | STN EN ISO 527-2 |
Plastcom PLASTAMID® 6 GF 25 002 PA6 reinforced with glass fiber PA 6 for injection molding, reinforced with 25% glass fiber, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, .. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | |
Plastcom SLOVAMID 66/6 GF 20 PA66/6, 20% glass fibre FeaturesChemically reinforced alloy PA 66 and PA 6 with 20 % glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and .. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | same value from ASTM and ISO test. |
BASF Capron® GR20 HS 20% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR20 HS is a heat stabilized 20% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest.. |
|||
Tensile Modulus | 7.00 GPa @Temperature 150 °C |
1020 ksi @Temperature 302 °F |
ISO 527 |
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded
(d AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, .. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | |
LATI Laticonther 87/28 GR/50 PC, 50% Graphite Reinforced High thermal conductivity product based on Polycarbonate (PC). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218HP V35 PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218HP V35 is a polyamide 6.6, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product of.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 Type 1A |
Solvay TECHNYL® B 218L V20 Black 44 N PA66, 25% glass fiber, DRY Description: Copolyamide 66/6, reinforced with 20% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistanceAvailable in: Asia Pacific and EuropeProduct Applications:.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® 3320GF Polyethersulfone (PESU), 20% Glass Fiber Veradel® 3320GF is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON PFD04ES PA 6 (Europe-Africa-Middle East) LNP* STATKON* PFD04ES is a compound based on PA 6 resin containing Carbon Powder, Glass Fiber. Added features include: Electrically Conductive, Easy Molding, Heat Stabilized. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
Polyram PlusTek PD300G5 Nylon 12 for Injection Molding, 25% Glass-Fiber Reinforced 25% Glass-fiber reinforced Nylon 12, heat stabilized and hydrolysis resistant for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527-1/-2 |
DSM Arnite® TV4 230 SF PBT-15% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 MRGV 20/10 HWCP 20% Mineral and 10% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® HT2V-15H PA6T/66-GF15 Product description: Grivory HT2V-15H is a 15 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-3 ESD PA12-GF30 Product description: Grilamid LV-3 ESD is an antistatic PA12 injection molding grade, with fiber reinforcement of 30%. Due to its special formulation, the material can be used for applications where.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® SK692FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK692FR is a 15% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided by .. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
Eurotec® Tecodur® PB70 GR30 NL IL PBT 30% glass fiber reinforced, impact modified Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
Eurotec® Tecopet® PT70 GR15 NL100 PS20 PET, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
Eurotec® Tecodur® PB70 GR20 NL PBT 20% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
Eurotec® Tecolen® CP20 GR40 NL PPCP, 40% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
Eurotec® Tecomid® MB40 GR20 NL PA6, 20% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527 |
Eurotec® Tecotek® PC30 GR20 GR003 ZG20 PC, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), grey RAL 7035 Information provided by Eurotec® |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527-1 |
Barlog Plastics KEBAFORM C 2027 POM Copolymer, 20% glass fiber reinforced POM-GF20Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® S3 GF 23 1 (2917) PA 6.10 Dry, 23% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | 1mm/min; ISO 527 |
BASF Ultradur S 4090 G4 LS High Speed BK15077 20% Glass Filled PBT |
|||
Tensile Modulus | 7.00 GPa | 1020 ksi | ISO 527-1-2 |
BASF Ultradur® B 4300 G4 FC 20% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |