Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.29 GPa | 1200 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP IX04513C PA 6/12 (Asia Pacific) LNP THERMOCOMP* IX04513C is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Clean Compounding System. |
|||
Tensile Modulus | 8.29 GPa | 1200 ksi | 1mm/min; ISO 527 |
BASF Ultramid® SEGM35 H1 BK-126 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid SEGM35 H1 BK-126 is a 40% glass/mineral reinforced injection molding grade. It offers enhanced surface appearance, it also exhibits similar UV weathering characteristics compared to 8267G .. |
|||
Tensile Modulus | 8.29 GPa | 1200 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP IX04513C PA 6/12 LNP THERMOCOMP* IX04513C is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Clean Compounding System. |