Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.75 GPa | 1120 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PX5558 PPE+PS 30% glass reinforced, high flow PPO. |
|||
Tensile Modulus | 7.75 GPa | 1120 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL EM7430 PPE+PS 30% glass reinforced, high flow PPO. Automotive. Energy management material. |
|||
Tensile Modulus | 7.75 GPa | 1120 ksi | ISO 527 |
Polyram Polytron P30N11 Polypropylene, 30% Long Fiber Glass A chemically coupled 30% long fiber glass reinforced natural polypropylene, heat stabilized, for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 7.75 GPa | 1120 ksi | ISO 527 |
Polyram Polytron P30B07 Polypropylene, 30% Long Glass Fibers, UV Stabilized A chemically coupled 30% long glass fibers reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 7.75 GPa | 1120 ksi | ASTM-D790 |
Polyram Polytron P30N01 Homopolymer Polypropylene, Chemically Coupled 30% Long Fiber A CHEMICALLY COUPLED 30% LONG FIBER GLASS REINFORCED NATURAL POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 7.75 GPa @Temperature -35.0 °C |
1120 ksi @Temperature -31.0 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |
|||
Tensile Modulus | 7.75 GPa | 1120 ksi | |
Radici Radilon® A RV300R (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Modulus | 7.75 GPa | 1120 ksi | ASTM-D790 |
Polyram Polytron P30B01 Homopolymer Polypropylene, Chemically Coupled 30% LGF A chemically coupled 30% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 7.75 GPa | 1120 ksi | ASTM-D790 |
Polyram Polytron P30B11 Homopolymer Polypropylene, Chemically Coupled 30% LGF A chemically coupled 30% LGF reinforced black PP, heat stabilized for injection molding applications.Information provided by Polyram Ram On Ind. |