Polymer Property : Tensile Modulus = 5.299 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 5.299 GPa
768.6 ksi
ASTM D638
Aclo Accutech ABS ABS832G30L Glass Reinforced
Tensile Modulus 5.299 GPa
768.6 ksi
ASTM D638
Aclo Accutech ABS ABS834G40L Glass Reinforced