Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® GPM5500U ABS (Europe-Africa-Middle East) CYCOLAC GPM5500U is a UV stabilized multi purpose injection moulding grade, providing a favourable balance of engineering properties. CYCOLAC GPM5500U has a wide processing window. It is recommended.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Asia Pacific) Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HP2REU PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a h.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® IFX5420Z PC (Asia Pacific) Lexan* IFX5420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grade meets the transmis.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® LUX9132C PC COPOLYMER (Asia Pacific) Lexan* LUX9132C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® CFR9131 PC COPOLYMER (Asia Pacific) Lexan* CFR9131 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and .. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DX11354X PC (Asia Pacific) LNP* Thermocomp* Compound DX11354X is a colorable PC based compound with stable plating and RF performance, colored LDS material solution, good surface and processing window, high impact strength. I.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | ISO Data. |
Styron Pulse® 1350 ABS + Polycarbonate PULSE® 1350 Engineering resin offers a superior total performance with a balance of heat resistance, practical toughness, high and low temperature impact strength retention and ease of processing.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PX5511E PPE+HIPS (Europe-Africa-Middle East) Noryl PX5511E is an unfilled material with good flow and chemical resistance against cleaners. Noryl PX5511E is developed for personal care appplications. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | ASTM-D790 |
Polyram RamTal PM340S4 Acetal, 20% Glass beads Reinforced 20% Glass beads reinforced polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | |
Covestro Bayblend® KU 2-1481 Polycarbonate/ABS Blend Increased thermal stability during processing, slightly higher modulus of elasticity and slightly decreased low-temperature toughness compared to BAYBLEND T 85 MN.Information provided by Bayer.As of.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | ISO 527-1/-2 |
Covestro Bayblend® KU 2-1514* Polycarbonate + ABS, Flame Retardant Grade Developmental productHigh heat resistant injection molding gradeball indentation temperature =125 °CVicat/B 120 temperature = 136 °CUL-listing 94 V-0 at 1.5 mmsuitable for supporting life componen.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | ISO 527-1/-2 |
Covestro Makrolon® 1804 Polycarbonate MVR (300 °C/1.2 kg) 6.0 cm3/10 minhigh viscosityUV stabilizedoptimized for low plate-outimproved flammabilityUL 94 V-2/1.5 mm and 3.0 mmavailable in transparenttranslucent and opaque colorssolid sh.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527-1,-2 |
Covestro Makrolon® 2405 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527-1,-2 |
Covestro Makrolon® 2405 MAS057 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527-1,-2 |
Covestro Makrolon® ET3117 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527-1,-2 |
Covestro Makrolon® FR6901 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Hig.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | ISO 527-1/-2 |
Covestro Makrolon® LQ3147 Polycarbonate ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minOptical lensHigh viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in clear tints .. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSZ 1 PA666 Product description: Grilon TSZ 1 is a heat stabilized, normal viscosity, impact modified PA66 + PA6 injection molding grade. Grilon TSZ 1 has the following important properties: Excellent flow beha.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FE3734 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612 Zytel FE3734 NC010 is an unreinforced lubricated polyamide 612 resin suitable for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | ISO 527 |
BASF Ultramid® 1C PA6/66 (Dry) Description: Ultramid® 1C forms flexible, scratch-resistant coatings or tough, resilient, abrasion-resistant coverings on plastics, films, nonwovens, fabrics, leather, paper, wood, or metal.Informa.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0339T40L1 Talc Reinforced |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 1mm/min; ISO 527 |
Borealis ME268Al Polypropylene Compound, Mineral Filled ME268AI is a 20% mineral filled polypropylene compound intended for injection molding. Applications: ME268AI has been developed especially for the car industry to be used in automotive interior par.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXALEN PPC339T20 Polypropylene Copolymer, 20% Talc Filled SAXALEN PPC339T20 is a 20% mineral filled Polypropylene - Copolymer intended for injection molding with good flow properties und higher stiffness. The PP-Copolymer has low warpage behaviors and good.. |
|||
Tensile Modulus | 2.40 GPa @Temperature 23.0 °C |
348 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Sorona® 3301 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)&l Sorona® 3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with superior surface appearance in ambient temperature conditions... |