Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.18 GPa | 316 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® EXL1464T PC Copolymer (Asia Pacific) Lexan* EXL1464T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® EXL1464T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1464T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer (Asia Pacific) Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb.. |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb.. |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXE1414T PC Copolymer (Asia Pacific) Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in ""Energy"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color pac.. |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Asia Pacific) 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HPF0 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HPF1 PC Copolymer 25 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® ML7647 PC Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque onlyThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® ML7647 PC (Asia Pacific) Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque only |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® ML7647 PC (Europe-Africa-Middle East) Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque onlyThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® ML7647K PC (Asia Pacific) Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque only |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL9414T PC Copolymer (Asia Pacific) Lexan* EXL9414T resin grade is a halogen-free flame retardant polycarbonate featuring transparency, -40 degree C ductility and UL-94 V0 rating for injection molding applications. Excellent impact co.. |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXE1414T PC Copolymer (Europe-Africa-Middle East) Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa.. |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Europe-Africa-Middle East) 40 MFR LEXAN High Flow Ductile Copolymer |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Europe-Africa-Middle East) 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL003EU PC LNP LUBRICOMP* DL003EU is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Easy Molding, UV Stabilized, Internally Lubricated. |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Asia Pacific) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Europe-Africa-Middle East) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXRL0672 PC Copolymer 40 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXE1434T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Asia Pacific) 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer |
|||
Tensile Modulus | 2.18 GPa | 316 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Asia Pacific) 40 MFR LEXAN High Flow Ductile Copolymer |