Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.137 GPa | 310.0 ksi | ASTM D638 |
Ineos Styrenics 495F High-Impact Polystyrene Resin (Global) Description: High-impact, high-flow grade for a wide variety of applications, including appliance components, consumer electronics housings, magnetic and optical media, building and construction, pa.. |
|||
Tensile Modulus | 2.137 GPa | 310.0 ksi | ASTM D638 |
Ineos Styrenics 496N High-Impact Polystyrene Resin (NAFTA) Description: High-impact, lower flow grades for food packaging, dairy containers, lids, plates, appliance components and housings.Information provided by BASF.Ineos Styrenics purchased this product .. |
|||
Tensile Modulus | 2.137 GPa | 309.9 ksi | Z; ASTM D638 |
ALM PA-840-GSL Filled Nylon 12 Prototyping Polymer Engineered for excellent mechanical properties, part definition and surface finish.Stabilized against thermal degradation resulting in little or no scrap material, with typical virgin refresh rates .. |