Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 17.2 GPa @Temperature 23.9 °C |
2500 ksi @Temperature 75.0 °F |
0° Direction, Dry; 8HS form; ASTM D638 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, ENKA Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
Tensile Modulus | 17.2 GPa @Temperature 23.9 °C |
2500 ksi @Temperature 75.0 °F |
0° Direction, Dry; 325°F Autoclave; ASTM D638 |
Park Electrochemical Nelcote® F-557 Phenolic Prepreg, Aerospace Silica Fabric Reinforced Nelcote® F-557 is a high purity silica filler phonic resin coated on Commercial or Aerospace grade silica fabric. F-557 is used in the manufacture of intermediate temperature ablative rocket nozzle.. |
|||
Tensile Modulus | 17.2 GPa @Temperature 23.9 °C |
2500 ksi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® F-562 Phenolic Prepreg, 8HS Silica Reinforced Nelcote® F-562 is an elastomer modified phenolic resin used in the manufacture of intermediate temperature ablative rocket nozzles, heat shields and combustion chambers in highly oxidative environm.. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Tensile Modulus | 17.2 GPa @Temperature 100 °C |
2490 ksi @Temperature 212 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica.. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | ASTM D638 |
Sumitomo Bakelite Durez® 23570 Phenolic, Compression Grade Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft.. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | ASTM D638 |
Sumitomo Bakelite Durez® 32245 Phenolic, Compression Grade Durez 32245 Black Phenolic is a two-stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional stabilit.. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | ASTM D638 |
Sumitomo Bakelite Durez® 32245 Phenolic, Injection Grade Durez 32245 Black Phenolic is a two-stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional stabilit.. |
|||
Tensile Modulus | 17.2 GPa | 2500 ksi | ASTM D638 |
Lubrizol ISOPLAST™ 2560 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaAvailableInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | ASTM-D790 |
Polyram Polytron A50B02 Nylon 66, Chemically Coupled 50% Long Fiber A CHEMICALLY COUPLED 50% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTIONInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | 5.0 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr.. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | ASTM-D790 |
Polyram Polytron A50N02 Nylon 66, Chemically Coupled 50% Long Fiber A CHEMICALLY COUPLED 50% LONG FIBER GLASS REINFORCED NATURAL NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTIONInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 17.2 GPa | 2500 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AM-20CF-20GF/000 Polyphthalamide (PPA), Glass/Carbon Fiber Filled
(discontinued **) Description/Features:Glass/Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |