Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 16.5 GPa | 2390 ksi | ISO 527, ASTM D638 |
Nilit Nilamid A3 H G10 50% Glass Reinforced PA66 Description: Nilamid A3 H G10 (50% Glass Reinforced) is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance,.. |
|||
Tensile Modulus | 16.5 GPa @Temperature 21.1 °C |
2400 ksi @Temperature 70.0 °F |
0° Direction, Dry; Vacuum/Oven Cured; ASTM D3039-95 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® NN-50GF/000 Polyamide 66 (Nylon 66) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PC-30CF/20T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | ISO 527-1/-2 |
DSM Akulon® Ultraflow™ K-FG0 Nylon 6-50% Glass Reinforced (European and Asian Grade) (Dry)
(discontinued **)& The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | ASTM D638 |
PolyOne LubriOne™ NJ-30CF/15T-2S Nylon 12
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 16.5 GPa | 2400 ksi | |
MTI ThermoStran® TPU-60G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® G4V-5H black 9915 PA*-GF50 Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® G4V-5H black 9915 PA*-GF50 Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GVL-5H nat PA*-GF50 Product description: Grivory GVL-5H natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H na.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HTV-45H1 black 9205 PA6T/6I-GF45 Product description: Grivory HTV-45H1 black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation a.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-50 PA666-GF50 Product description: Grilon TSG-50 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50 has the following important properties: High stiffne.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-50/4 W PA666-GF50 Product description: Grilon TSG-50/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4116 black 9288 PA1010-GF55 Product description: Grilamid XE 4116 black 9288 is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, paint.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4116 nat PA1010-GF55 Product description: Grilamid XE 4116 natural is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, painted .. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | ISO 527-1 |
Barlog Plastics KEBATER A9045 PBT, 45% glass fiber reinforced, improved surface quality, reduced warpage, food grade (PBT+X)-GF45Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Conditioned, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, at 50% RH
& Data provided by the manufacturer, Amoco Corporation.AMODEL AF-1550 V0 resin is a 50% glass/mineral reinforced, flame retarded polyphthalamide (PPA) that features: high deflection temperature, high .. |