Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527-2 |
PolyOne OnForce™ LFT LF9200-5001 RS Natural Polyphenylene Sulfide (PPS) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527-2 |
PolyOne OnForce™ LFT NN-40LGF/000 HS UV Black Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ASTM D638 |
Premix Premi-Glas® 1281-47 VE SMC Description: Premi-Glas® 1281-47 VE is a sheet molding compound.Market: StructuralInformation provided by Premix. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 V40 Black 21 NHFE PA66, 40% glass fiber, DRY Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 40% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECH.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RC003 PA 66 (Europe-Africa-Middle East) 15% carbon fibre reinforced Polyamide 66 injection moulding resin. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527-1/-2 |
Unitika RUN35-C25 PA6, Conditioned High modulus and low warpage nylonInformation provided by Unitika Ltd. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ASTM-D790 |
Polyram Polytron P60B04 Homopolymer Polypropylene, Chemically Coupled 60% Long Glass Fiber A CHEMICALLY COUPLED PP 60% LONG GLASS FIBER WITH EXTRA LOAD OF ADDITIVES FOR DILUTION.Information provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527 |
Vyncolit 4421 XB Novolac Phenolic Mineral and organic filled phenolic molding compound with good mechanical properties.USES: Fuse holders, brush holders, circuit breakers, automotive ignition and solenoid covers.Information provided.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527-1/-2 |
DSM Arnite® AV2 370 /B PET-35% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | dry; ISO 527-1/-2 |
DSM Stanyl® TE200F8 PA46-GF40 40% Glass Reinforced, Heat Stabilized, for E&E applications |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | dry; ISO 527-1/-2 |
DSM Stanyl® TS241B3 PA46-CF15 15% Carbon Reinforced, Lubricated |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527-1/-2 |
DSM Stanyl® TW200F8 Nylon 46-40% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-4 FWA nat PA*-GF40 Product description: Grivory GV-4 FWA natural is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GVL-4H nat PA*-GF40 Product description: Grivory GVL-4H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 40% long glass fibers. Grivory GVL-4H blac.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGL-40/4 nat PA666-GF40 Product description: Grilon TSGL-40/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 natural is characterized by the following .. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 5106 (GVL-4H V0) PA*-GF40 Product description: Grivory XE 5106 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinf.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527 |
Eurotec® Tecomid® NA40 GR40 NL RM PA6.6, 40% glass fiber reinforced, MoS2 modified, natural Information provided by Eurotec® |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527-1/-2 |
DSM Arnite® AV2 360 S PET-33% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527-1/-2 |
DSM Arnite® AV2 370 HF PET-GF35 35% Glass Reinforced, Brake Booster Body Valves, High Flow |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527-1/-2 |
DSM Arnite® AV2 372 PET-35% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-4H PA*-GF40 Product description: Grivory GV-4H natural is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide... |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4217 black 9233 PA6T/66-GF45 Product description: Grivory XE 4217 black 9233 is a high heat stabilized, 45% glass fiber reinforced, semicrystalline, thermoplastic engineering material for injection moulding. Polymer designation.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527 |
Eurotec® Tecopet® PT70 GR30 NL100 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® T6 GF 40 (3500) PPA Conditioned, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-4H black PA*-GF40 Product description: Grivory GV-4H black 9915 is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Tensile Modulus | 13.0 - 15.0 GPa | 1890 - 2180 ksi | ISO 527 |
Vyncolit 3520 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |