Polymer Property : Tensile Modulus = 12.44 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 12.44 GPa
1804 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP UF006H PPA
LNP* THERMOCOMP* UF006H is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare.
Tensile Modulus 12.44 GPa
1804 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP UF006H PPA (Asia Pacific)
LNP* Thermocomp* UF006H is a compound based on Polyphthalamide resin containing Glass Fiber.