Mechanical Properties Metric English Comments
Tensile Modulus >= 0.115 GPa
>= 16.7 ksi
2% sec, MD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4118Q (18403) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus >= 0.115 GPa
>= 16.7 ksi
2% sec, MD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 5118Q (18603) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus 0.115 GPa
16.7 ksi
average; in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® C70.130 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negli..
Tensile Modulus 0.115 GPa
16.7 ksi
ISO 527
Gromax 1140LH TPE
Product Description: 1140LH is Low modulus grade with nominal Durometer hardness of 40D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like inject..
Tensile Modulus 0.115 GPa
16.7 ksi
ISO 527-1/-2
DSM Arnitel® EB463 41 Shore D, Blow Molding Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Modulus 0.115 GPa
16.7 ksi
ISO 527-1/-2
DSM Arnitel® EB463 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Modulus 0.115 GPa

@Temperature 150 °C
16.7 ksi

@Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo..
Tensile Modulus 0.115 GPa
16.7 ksi
1 mm/min
Arkema Group Evatane® 1005 VN 3 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for flexible, very transparent film with high strength, shrinking at low temperature. Examples: curtain stretch, coextrusion, ..
Tensile Modulus 0.115 GPa
16.7 ksi
ISO 527-1/-2
DSM Arnitel® EB464 42 Shore D, Blow Molding Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Modulus 0.115 GPa
16.7 ksi
ISO 527-1/-2
DSM Arnitel® EB464 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..