Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 0.0300 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.0300 GPa
4.35 ksi
ISO 527-1/-2
DuPont Performance Polymers Hytrel® SC948 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for the Healthcare Industry Hytrel SC948 NC010 is a low modulus grade with nom. durometer hardness of 40D contains non-discoloring stabilize..
Tensile Modulus 0.0300 GPa
4.35 ksi
average; in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® R63.50 Damage Tolerant Foam
AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with high damage tolerance. This one of a kind formula combines very high elongation and excellent bond strength. AIREX® R63 is cold..
Tensile Modulus >= 0.0300 GPa
>= 4.35 ksi
ASTM D4745-97
Adamas Adalon® 413 PTFE, 20% PPS
Information provided by Adamas, HPM
Tensile Modulus 0.0300 GPa
4.35 ksi
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Tensile Modulus >= 0.0300 GPa
>= 4.35 ksi
in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® C71.55 Elevated Temperature Structural Foam
AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength..