Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 370 - 560 MPa | 53700 - 81200 psi | |
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; H (TD04) Temper; up to 76 mm Thickness (UNS C17500) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 480 - 560 MPa | 69600 - 81200 psi | Solution Annealed and Aged |
Materion Beryllium Copper Alloy 10C Castings (UNS C82000) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchTabul.. |
|||
Tensile Strength, Yield | 410 - 560 MPa | 59500 - 81200 psi | |
Materion Beryllium Copper Alloy 25 Strip; 1/4 H (TD01) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): 0Superficial Hardness: 30T 62-75Tabulated properties apply .. |
|||
Tensile Strength, Yield | 510 - 560 MPa | 74000 - 81200 psi | L direction |
ArcelorMittal Speed 35-510 Electrical Steel Properties: The iCARe™ Speed product family comes with guaranted losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 370 - 560 MPa | 53700 - 81200 psi | |
Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; H (TD04) Temper; up to 76 mm Thickness (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |