Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 20.0 - 34.0 MPa | 2900 - 4930 psi | ASTM D638 |
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Tensile Strength, Yield | 20.0 - 34.0 MPa | 2900 - 4930 psi | ASTM D638 |
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s.. |
|||
Tensile Strength, Yield | 20.0 - 34.0 MPa | 2900 - 4930 psi | ASTM D638 |
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Tensile Strength, Yield | 24.0 - 34.0 MPa | 3480 - 4930 psi | ASTM D638 |
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Tensile Strength, Yield | 24.0 - 34.0 MPa | 3480 - 4930 psi | ASTM D638 |
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Tensile Strength, Yield | 1.80 - 34.0 MPa | 261 - 4930 psi | Average value: 14.0 MPa Grade Count:39 |
Overview of materials for Polyether Block Amide (PEBA) This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a.. |
|||
Tensile Strength, Yield | 20.0 - 34.0 MPa | 2900 - 4930 psi | ASTM D638 |
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |