Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 650 - 870 MPa | 94300 - 126000 psi | |
Materion Beryllium Copper Alloy 10 Rod and Bar; HT (TH04) Temper; up to 76 mm (UNS C17500) Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Yield | 650 - 870 MPa | 94300 - 126000 psi | |
Materion Beryllium Copper Alloy 10 Wire; HT (TH04) Temper; 1.3-12.7 mm Diameter (UNS C17500) Treatment required for max strength: 2 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Tensile Strength, Yield | 650 - 870 MPa | 94300 - 126000 psi | |
Materion Beryllium Copper Alloy 174 Strip; HT (TH04) Temper (UNS C17410) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 95%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R.. |
|||
Tensile Strength, Yield | 650 - 870 MPa | 94300 - 126000 psi | |
Materion Beryllium Copper Alloy 190 Strip; 1/2HM (TM02) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R.. |
|||
Tensile Strength, Yield | 689 - 869 MPa | 99900 - 126000 psi | 0.2% proof |
Kobe Steel KS15-3-3-3 Beta Titanium Alloy, AMS 4914, Solution treated Nominal Composition: Ti-15 V-3 Cr-3 Sn-3 AlApplications: Aircraft parts, bicycle gears, gold club heads, foils. Features:Cold workable.Information provided by Kobe Steel |
|||
Tensile Strength, Yield | 620 - 870 MPa | 89900 - 126000 psi | |
Materion Beryllium Copper Alloy 25 Wire; 1/2H (TD02) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 650 - 870 MPa | 94300 - 126000 psi | |
Materion Beryllium Copper Alloy 3 Rod and Bar; HT (TH04) Temper; up to 76 mm (UNS C17510) Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Yield | 620 - 870 MPa | 89900 - 126000 psi | |
Materion Beryllium Copper Alloy M25 Wire; 1/2H (TD02) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 650 - 870 MPa | 94300 - 126000 psi | |
Materion Beryllium Copper Alloy 3 Tube; HT (TH04) Temper; up to 76 mm o.d. (UNS C17510) Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc... |
|||
Tensile Strength, Yield | 650 - 870 MPa | 94300 - 126000 psi | |
Materion Beryllium Copper Alloy 3 Wire; HT (TH04) Temper; 1.3-12.7 mm Diameter (UNS C17510) Treatment required for max strength: 2 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials .. |