Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 52.4 - 79.3 MPa | 7600 - 11500 psi | Average value: 63.6 MPa Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |
|||
Tensile Strength, Yield | 13.0 - 79.0 MPa @Temperature -40.0 - 80.0 °C |
1890 - 11500 psi @Temperature -40.0 - 176 °F |
Average value: 45.9 MPa Grade Count:5 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Tensile Strength, Yield | 29.0 - 79.3 MPa | 4210 - 11500 psi | Average value: 53.2 MPa Grade Count:19 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Tensile Strength, Yield | 20.0 - 79.3 MPa | 2900 - 11500 psi | Average value: 35.6 MPa Grade Count:21 |
Overview of materials for Nylon, Flexible Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri.. |