Mechanical Properties Metric English Comments
Tensile Strength, Yield 6.50 MPa
943 psi
ASTM D412
Polymax® Maxelast® P3672 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 6.50 MPa
943 psi
ISO 527
Polimeri Europa Greenflex® ML 30 Ethylene Vinyl Acetate Copolymer - Injection Molding & Profile Extrusion
Greenflex ML 30 is an ethylene vinyl acetate copolymer (EVA) for injection molding and profile extrusion. Items produced with Greenflex ML 30 show good ESCR and elasticity.Main Applications: Green..
Tensile Strength, Yield 6.50 MPa
943 psi
ISO 527
Polimeri Europa Greenflex® ML 31 Ethylene Vinyl Acetate Copolymer - Injection Molding & Profile Extrusion
Greenflex ML 31 is an ethylene vinyl acetate copolymer (EVA) for injection molding applications and extrusion profile. Greenflex ML 31 contains additive waxes to obtain high production speed.Main A..
Tensile Strength, Yield 6.50 MPa
943 psi
ASTM D412
Precision Polymer Engineering F80R Fluorosilicone Rubber
Red Fluorosilicone, 76-85 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification DTD5583A Grade 80.Applications:
Tensile Strength, Yield 6.50 MPa
943 psi
ASTM D412
Precision Polymer Engineering S80D Silicone Rubber
Black Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ. Formulated to meet UK Ministry of Defence ..
Tensile Strength, Yield 6.50 MPa

@Temperature 100 °C
943 psi

@Temperature 212 °F
ASTM D638
Micropol Isoplas P501 Crosslinkable Polyethylene
Information provided by Micropol Limited
Tensile Strength, Yield 6.50 MPa
943 psi
ASTM D412
Vicone High Performance Rubber VicoSil™ C303Q-GY High Performance Silicone Rubber
Information provided by Vicone
Tensile Strength, Yield 6.50 MPa
943 psi
Trelleborg B419 Nitrile Rubber
Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi..
Tensile Strength, Yield 6.50 MPa
943 psi
Trelleborg B573 Nitrile Rubber
Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi..
Tensile Strength, Yield 6.50 MPa
943 psi
Trelleborg Neoprene® C423 Chloroprene
CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade..
Tensile Strength, Yield 6.50 MPa
943 psi
Trelleborg S561 Silicone Rubber
PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering...
Tensile Strength, Yield 6.50 MPa
943 psi
Trelleborg S562 Silicone Rubber
PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering...
Tensile Strength, Yield 6.50 MPa
943 psi
Trelleborg S565 Silicone Rubber
PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering...
Tensile Strength, Yield 6.50 MPa
943 psi
Trelleborg Commercial Neoprene® C801 Chloroprene
CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade..
Tensile Strength, Yield 6.50 MPa
943 psi
ASTM D638
Arkema Group OREVAC® 18365-S Grafted Maleic Anhydride Polyethylene
OREVAC 18365-S is a grafted maleic anhydride polyethylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC 18365-S is mainly used in multi-layer tube to have good adhesion between..
Tensile Strength, Yield 6.50 MPa
943 psi
50 microns film; ASTM D882
Arkema Group Orevac® 9309 Film EVA-MAH Terpolymer
EVA Terpolymers based Main Application: Cast film coextrusionInformation provided by Arkema Group
Tensile Strength, Yield 6.50 MPa
943 psi
50 mm/min
Arkema Group Evatane® 1020 VG 3 Ethylene Vinyl Acetate
EVA copolymer made by high process tubular process. Applications Grade for transparent films, high strength, sealing at low temperature, hot tack. Examples: laminates, coextrusion, secondary sealing..
Tensile Strength, Yield 6.50 MPa
943 psi
50 mm/min
Arkema Group Evatane® 1020 VN 3 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for flexible, very transparent films with high strength, very good sealability. Examples: thin stretch film for food packaging..
Tensile Strength, Yield 6.50 MPa
943 psi
Trelleborg Commercial Neoprene® C433 Chloroprene
CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade..