Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Trelleborg S562 Silicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Trelleborg
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg S562 Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering.Exhibits low flammability and low smoke toxicity.Good electrical insulation properties.Silicone rubber is physiologically inert, thus making it the preferred choice of the medical, pharmaceutical and food processing industries.Silicones have comparatively low mechanical properties, tensile strength, elongation and tear strength, however they keep constant even at high temperatures but should not be used with high pressure steam.Resistance to chemicals; its resistance to oils and hydrocarbon products is fairly limited and similar to that of Chloroprene rubbers. Reasonable resistance to a whole range of general chemical products, but acids, alkalis, esters and ketones should be avoided.All information provided by Trelleborg
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
Tensile Strength, Yield 6.50 MPa
943 psi
Elongation at Break 300 %
300 %
Tear Strength 17.0 kN/m
97.0 pli
Compression Set 45 %

@Temperature 70.0 °C,
Time 79200 sec
45 %

@Temperature 158 °F,
Time 22.0 hour
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Descriptive Properties Value Comments
Color Red
Users viewing this material also viewed the following: