Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Omni Plastics OmniTech™ ABS GRC10 NA Glass Reinforced OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and .. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Polymer Resources PC-HM-FR1-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Polymer Resources PC-HM-FR1-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Polymer Resources PC-HM-FR2-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Polymer Resources PC-HM-FR2-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Polymer Resources PCSF-FR Polycarbonate, 5% Glass Reinforced Structural Foam Grade Polycarbonate, 5% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing cond.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Polymer Resources PC-HM-FR1-[color]-TFE Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear Resistant Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Polymer Resources PC-HM-FR2 Polycarbonate, 10% Glass Reinforced, Flame Retardant Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Polymer Resources PC-HM-FR2-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Tensile Strength, Yield | 55.8 - 172 MPa | 8100 - 24900 psi | Average value: 79.1 MPa Grade Count:46 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Techmer ES Elastoblend® PA6/66 IM 6040 MB Availability: North AmericaForms: PelletsAdditive: Nucleating Agent, Heat Stabilizer, Lubricant and Impact ModifierFeatures: Copolymer, Nucleated, Heat Stabilized, Lubricant and Impact ModifiedInfor.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Techmer ES Electrablend® PC/ABS Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Electrically Conductive and ESD ProtectionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Techmer ES Electrablend® PC/ABS 033009 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Electrically Conductive and ESD ProtectionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6 FR 344 Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and LubricatedAppearance: RedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Techmer ES HiFill® HDPE GF30 A1 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Techmer ES Luriblend® PA6 TL25 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (25%)Features: Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4410-11 MFR Polycarbonate EMERGEâ„¢ PC 4410-11 advanced resin is a high impact polycarbonate resin designed for Information Technology Equipment and Injection Molding Applications.Information provided by DowThis product l.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Styron CALIBREâ„¢ IM 401-11 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D-638 |
Axiall ProTherm® 4510 CPVC Rigid PVC, Molding Georgia Gulf ProTherm® 4510 CPVC is a pelletized injection molding compound designed for fittings. Typical applications are in potable water and chemical transfer systems especially where high che.. |
|||
Tensile Strength, Yield | 55.8 - 145 MPa | 8100 - 21000 psi | Average value: 83.2 MPa Grade Count:10 |
Overview of materials for Nylon 6, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6 FR 344 BK Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |