Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 517 MPa @Temperature 23.9 °C |
75000 psi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D638 Type 1 |
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Aramid Reinforced Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f.. |
|||
Tensile Strength, Yield | 517 MPa | 75000 psi | |
Performance Alloys MoldStar® 150 (PAS 940) Copper Mold Alloy Description: MoldStar® 150 is a high-performance, beryllium-free copper alloy for the blow molding and injection molding industries. In addition to its high thermal conductivity, MoldStar® 150 off.. |
|||
Tensile Strength, Yield | 517 MPa | 75000 psi | |
Kennametal Stellite Stellite® 21 Excellent high temperature strength, high toughness. Solution treat at 1191-1204°C, rapid air cool, age between 538-871°C to increase hardness and strength at the expense of impact and ducti.. |
|||
Tensile Strength, Yield | 517 MPa @Strain 0.200 %, Temperature 538 °C |
75000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Kennametal Stellite Stellite® 6K 12.7 or 22.2 mm plate 13.3 mm^3 volume loss--abrasive wear data. Applications include agitators, augers, ball mills, banbury mills, cams, crusher bearings, dryers, dry presses, dump cars, fans, filters, food machinery, g.. |
|||
Tensile Strength, Yield | 517 MPa | 75000 psi | Annealed |
Kinetics MIM F1537 (ASTM F1537) HIP and Heat Treat Most commonly used within the medical market on applications requiring these characteristics: Bio-compatibility Corrosion resistance High strength Nonmagnetic Wear resistance. Information prov.. |
|||
Tensile Strength, Yield | 517 MPa | 75000 psi | |
Meehanite Almanite® WSH Wear and Abrasion Resisting Cast Iron Type WSH is an austenitic nodular iron possessing superior tensile strength, toughness and ability to work harden under conditions of severe pounding impact. It is extremely difficult to machine. .. |
|||
Tensile Strength, Yield | 517 MPa | 75000 psi | Stress relieved |
Special Metals MONEL® 404 Copper-Nickel Alloy Data provided by California Fine Wire and the manufacturer, Special Metals. |
|||
Tensile Strength, Yield | >= 517 MPa | >= 75000 psi | 1400°F for 2 hrs and 1150°F for 4 hrs |
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect.. |
|||
Tensile Strength, Yield | >= 517 MPa | >= 75000 psi | 0.2% Offset |
Eagle Brass 301 Austenitic Stainless Steel, 1/4 Hardened Type 301 is a chromium-nickel stainless steel that provides high strength and good ductility with chromium and nickel contents lowered to increase the work hardening range. This permits higher tens.. |
|||
Tensile Strength, Yield | >= 517 MPa | >= 75000 psi | 0.2% Offset |
Eagle Brass 305 Austenitic Stainless Steel, 1/4 Hardened Type 305 is a chromium nickel stainless steel that can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is nonmagnetic under most conditions. .. |
|||
Tensile Strength, Yield | >= 517 MPa | >= 75000 psi | 0.2% Offset |
Eagle Brass 316 Austenitic Stainless Steel, 1/4 Hardened The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 .. |
|||
Tensile Strength, Yield | >= 517 MPa | >= 75000 psi | 0.2% Offset |
Eagle Brass 316L Austenitic Stainless Steel, 1/4 Hardened Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a.. |
|||
Tensile Strength, Yield | 517 - 655 MPa | 75000 - 95000 psi | 0.2% Offset |
Eagle Brass 430 Ferritic Stainless Steel, 1/2 Hardened Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro.. |
|||
Tensile Strength, Yield | >= 517 MPa | >= 75000 psi | 0.2% offset |
Eagle Brass 7026 Copper Nickel, 1/4 Hard 7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company |
|||
Tensile Strength, Yield | >= 517 MPa | >= 75000 psi | 0.2% offset |
Eagle Brass 70265 XP175, 1/4 Hard Information provided by Eagle Brass Company |
|||
Tensile Strength, Yield | 517 - 621 MPa | 75000 - 90000 psi | 0.2% offset |
Eagle Brass 752 Nickel Silver 18%, Hard Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Tensile Strength, Yield | 517 MPa @Strain 0.200 % |
75000 psi @Strain 0.200 % |
|
ECOMold 135 Copper Mold Material ECOMold® copper alloys (beryllium-free) are engineered specifically for plastics industry applications. ECOMold® 135 has superior thermal conductivity compared to other common mold materials. T.. |
|||
Tensile Strength, Yield | 517 MPa | 75000 psi | |
CMW® 1000 AMS-T-21014 AMS-7725 ASTM B777 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |
|||
Tensile Strength, Yield | >= 517 MPa | >= 75000 psi | 0.2% Offset |
Eagle Brass 304L Austenitic Stainless Steel, 1/4 Hardened Type 304L is a very common variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled. Lower carbon 304L minimizes chromium ca.. |
|||
Tensile Strength, Yield | 517 - 586 MPa @Strain 0.200 % |
75000 - 85000 psi @Strain 0.200 % |
|
Ametek AM 388™ Alloy (UNS C72650) TD03 3/4 Hard Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Tensile Strength, Yield | 517 MPa | 75000 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 10% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Tensile Strength, Yield | 517 MPa @Strain 0.200 % |
75000 psi @Strain 0.200 % |
|
ATI Allvac® 35N Nickel Superalloy, Heat Treatment: 1052°C (1925°F) + Age Data provided by Allvac.Applications: Aircraft fasteners. Line wire for down-hole instrumentation. Biomedical devices, high fatigue strength applications. |
|||
Tensile Strength, Yield | 517 MPa @Strain 0.200 % |
75000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® H-W Nickel Superalloy, Heat Treatment: 1185°C (2165°F) Anneal Data provided by Allvac.Applications: Aerospace rings, forgings, weld wire. |
|||
Tensile Strength, Yield | 517 MPa @Strain 0.200 % |
75000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® N-90 Nickel Superalloy, Heat Treatment: 1066°C (1950°F) + Age Data provided by Allvac.Applications: Turbine blades and other jet engine components. Valves for internal combustion engines. |
|||
Tensile Strength, Yield | >= 517 MPa @Strain 0.200 % |
>= 75000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Stainless Steel Type 301, 1/4 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Tensile Strength, Yield | 517 MPa | 75000 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 10% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Tensile Strength, Yield | 517 MPa @Strain 0.200 % |
75000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 704°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Tensile Strength, Yield | 517 MPa @Strain 0.200 % |
75000 psi @Strain 0.200 % |
|
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 10% Cold Work Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®.. |