Polymer Property : Tensile Strength, Yield = 59500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 410 - 560 MPa
59500 - 81200 psi
Materion Beryllium Copper Alloy 25 Strip; 1/4 H (TD01) Temper (UNS C17200)
Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): 0Superficial Hardness: 30T 62-75Tabulated properties apply ..
Tensile Strength, Yield 410 MPa

@Strain 0.200 %
59500 psi

@Strain 0.200 %
Haynes 556® alloy, bar, after 1000 hours at 650°C (1200°F)
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Tensile Strength, Yield 410 MPa

@Strain 0.200 %
59500 psi

@Strain 0.200 %
Haynes 556® alloy, bar, after 8000 hours at 650°C (1200°F)
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Tensile Strength, Yield 410 MPa

@Strain 0.200 %
59500 psi

@Strain 0.200 %
Haynes 556® alloy, cold rolled, solution annealed sheet, 0.8-2.8 mm thick
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Tensile Strength, Yield 410 MPa

@Strain 0.200 %
59500 psi

@Strain 0.200 %
Solution Annealed. Value at room temperature
Special Metals NIMONIC® Alloy 86
A nickel-chromium-molybdenum alloy with a rare-earth (cerium) addition. It combines good formability and weldability with exceptional resistance to oxidation and scaling at temperatures to 1920°..
Tensile Strength, Yield >= 410 MPa
>= 59500 psi
AK Steel ASTM A 607 Class 1 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA)
ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec..
Tensile Strength, Yield >= 410 MPa
>= 59500 psi
AK Steel ASTM A 607 Class 2 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA)
ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. ..
Tensile Strength, Yield >= 410 MPa
>= 59500 psi
AK Steel ASTM A 715 Class 2 Formable, Grade 60F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA)
ASTM A 715 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. ..
Tensile Strength, Yield >= 410 MPa
>= 59500 psi
AK Steel SAE J1392, Grade 60F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA)
AK Steel Formable Grade - F indicates inclusion controlled low alloy.Information provided by AK Steel
Tensile Strength, Yield 410 - 450 MPa
59500 - 65300 psi
L direction
ArcelorMittal Save 20-13 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 410 - 450 MPa
59500 - 65300 psi
T direction
ArcelorMittal Save 20-15 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 410 - 450 MPa
59500 - 65300 psi
L direction
ArcelorMittal Save 25-14 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 410 - 450 MPa
59500 - 65300 psi
T direction
ArcelorMittal Save 25-16 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 410 - 450 MPa
59500 - 65300 psi
L direction
ArcelorMittal Save 27-15 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 410 - 450 MPa
59500 - 65300 psi
T direction
ArcelorMittal Save 27-17 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 410 - 450 MPa
59500 - 65300 psi
L direction
ArcelorMittal Save 30-15 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 410 - 450 MPa
59500 - 65300 psi
T direction
ArcelorMittal Save 30-17 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Yield 410 - 510 MPa
59500 - 74000 psi
ArcelorMittal TRIP 690 Very high strength steel, Cold Rolled Steel
Available in the following: uncoated (HCT690T), electrogalvanized (HCT690T+ZE) and Extragal®/Galvannealed (HCT690T+Z)Description: TRIP steels offer an outstanding combination of strength and ductil..
Tensile Strength, Yield >= 410 MPa
>= 59500 psi
AK Steel ASTM A 1011, Class 2 Formable, Grade 60F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F)
Information provided by AK Steel
Tensile Strength, Yield >= 410 MPa
>= 59500 psi
AK Steel ASTM A 1011, Class 2 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA)
Information provided by AK Steel