Mechanical Properties Metric English Comments
Tensile Strength, Yield 370 - 560 MPa
53700 - 81200 psi
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; H (TD04) Temper; up to 76 mm Thickness (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Yield 370 - 520 MPa
53700 - 75400 psi
Materion Beryllium Copper Alloy 10 Wire; H (TD04) Temper; 1.3-12.7 mm Diameter (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Yield 370 MPa

@Strain 0.200 %
53700 psi

@Strain 0.200 %
Haynes 230® alloy, plate, 1000 hours exposure at 871°C (1600°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Tensile Strength, Yield 370 MPa

@Strain 0.200 %
53700 psi

@Strain 0.200 %
Haynes 556® alloy, sheet after 1000 hours at 648°C
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Tensile Strength, Yield 370 MPa

@Strain 0.200 %
53700 psi

@Strain 0.200 %
Haynes 556® alloy, sheet after 1000 hours at 760°C (1400°F)
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Tensile Strength, Yield 370 MPa

@Strain 0.200 %
53700 psi

@Strain 0.200 %
Haynes 625 alloy, 20% cold reduction, 1175°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Tensile Strength, Yield 370 MPa

@Strain 0.200 %,
Temperature 540 °C
53700 psi

@Strain 0.200 %,
Temperature 1000 °F
Haynes 625 alloy, cold rolled and 1050°C mill-annealed sheet
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Tensile Strength, Yield 370 MPa

@Strain 0.200 %,
Temperature 650 °C
53700 psi

@Strain 0.200 %,
Temperature 1200 °F
Haynes 625 alloy, cold rolled and 1050°C mill-annealed sheet
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Tensile Strength, Yield 370 MPa

@Strain 0.200 %
53700 psi

@Strain 0.200 %
Annealed prior to test
Special Metals BRIGHTRAY® Alloy F Electrical Resistance Alloy
A nickel-iron-chromium electrical-resistance alloy for use at temperatures up to 1920°F (1050°C) under continuous operating conditions. Its high iron content and relatively low level of nicke..
Tensile Strength, Yield 370 MPa
53700 psi
SSAB Tunnplat Domex® 034 BOR Rolled Boron Steel
Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron ..
Tensile Strength, Yield 370 MPa

@Temperature 23.0 °C
53700 psi

@Temperature 73.4 °F
90º, Wet; EN2561
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber
Information provided by HexCel
Tensile Strength, Yield >= 370 MPa
>= 53700 psi
Guaranteed minimum; long transverse
Alcoa 2324-T39 Aluminum Plate
Alloy 2324-T39 is a higher strength version of alloy 2024-T351 and is a purity controlled composition variant of alloy 2024. It was developed for tension-dominated, fatigue and fracture critical pl..
Tensile Strength, Yield >= 370 MPa

@Strain 0.200 %
>= 53700 psi

@Strain 0.200 %
CLAL-MSX ARCAP Anticorrosion AP1 H12 1/2 hard, Rolled Copper Alloy
Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin..
Tensile Strength, Yield <= 370 MPa

@Strain 0.200 %
<= 53700 psi

@Strain 0.200 %
CLAL-MSX DECLAFOR® 1015 TB Wire quenched Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Tensile Strength, Yield 370 - 480 MPa

@Strain 0.200 %
53700 - 69600 psi

@Strain 0.200 %
CLAL-MSX DECLAFOR® 1015 TD1 Rod quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Tensile Strength, Yield 370 - 480 MPa

@Strain 0.200 %
53700 - 69600 psi

@Strain 0.200 %
CLAL-MSX DECLAFOR® 1015 TD1 Wire quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Tensile Strength, Yield 370 - 520 MPa
53700 - 75400 psi
Materion Beryllium Copper Alloy 3 Wire; H (TD04) Temper; 1.3-12.7 mm Diameter (UNS C17510)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Yield 370 - 560 MPa
53700 - 81200 psi
Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; H (TD04) Temper; up to 76 mm Thickness (UNS C17510)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Copyright © lookpolymers.com All Rights Reserved