Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 26.2 MPa | >= 3800 psi | ASTM D638 |
S&E Specialty Polymers GPP6100-116C PP Application: Specially engineered, low bloom, low specific gravity, flame retardant polypropylene compound designed with halogen based technology. Exhibits a unique balance of high flexural modulus .. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | Type 1 bar; ASTM D638 |
Network Polymers Softflex® UB 30 Black OEX Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
Chevron Phillips HiD® 9055 HDPE Injection Molding Resin
(discontinued **) Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 231, A 52600Characteristics: Excellent Flow, Moderate Impact Strength, Good Stiffness, Moderate ESCR, Excellent Shrinkage ResistanceAppli.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
Chevron Phillips HiD® 9404 HDPE Blow Molding Resin
(discontinued **) Resin Type: linear copolymerCharacteristics: medium molecular weight distributions, wide range of processing conditions, low parison sag, good stress crack resistance. Federal specification LP390C .. |
|||
Tensile Strength, Yield | >= 26.2 MPa | >= 3800 psi | ASTM D 638 type IV |
Total Finathene® CD 522 HDPE corrugated pipe resin
(discontinued **) Applications: corrugated pipe, storm and sanitary sewers, drainage systemsInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics produc.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with DOP Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
LyondellBasell Petrothene® LT570401 High Density Polyethylene ApplicationsPETROTHENE LT 5704-01 resin exhibits good stiffness and environment stress crack resistance. Typical applications are bleach and household chemical bottles.Regulatory StatusLT 5704-01 m.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
Fiberfil® PP-61/TC/20/UV Polypropylene Copolymer, 20% Talc, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
Flint Hills 43S2A Polypropylene Random Copolymer Features: Good clarity.Applications: Film extrusion and blow moldingInformation Provided by Flint Hills Resources |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
Techmer ES HiFill® PP 0225 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
Techmer ES HiFill® PP 0254 S Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | At 50 mm/min; ASTM D638 |
Borealis Bormed™ RB845MO Random Copolymer for Healthcare Applications Bormed RB845MO is a random copolymer for blow molding with very good transparency and high contact clarity, very good gloss and surface finish. Bottles in sizes up to 2 quarts molded from Bormed RB.. |
|||
Tensile Strength, Yield | >= 26.2 MPa | >= 3800 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ FPP 2121UV-M-31 Black Filled Polypropylene Homopolymer DescriptionPolyfort® FPP 2121UV-M-31 is a 30% black filled polypropylene homopolymer. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman... |
|||
Tensile Strength, Yield | >= 26.2 MPa | >= 3800 psi | ASTM D 638 type IV |
Total 50100.2 HDPE blow molding, sheet, thermoforming resin Applications: Agricultural chemical tanks, portable fuel containers, industrial parts, pallets, large foam parts, food packaging, sheet extrusion, thermoforming, truck bed liners, dunnage containers.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® 6502A Blow Molding and Injection Molding Polypropylene Impact CopolymerApplications: Blow molded bottles and containers, blown and cast film applications, and profile extrusions.Formolene 6502A is a medium impact copolymer with an excellent balance of t.. |
|||
Tensile Strength, Yield | >= 26.2 MPa | >= 3800 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ FPP 2121UV-M-31 Black Filled Polypropylene Homopolymer DescriptionPolyfort® FPP 2121UV-M-31 is a 30% black filled polypropylene homopolymer. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman... |
|||
Tensile Strength, Yield | >= 26.2 MPa | >= 3800 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ FPP 2121UV-M-31 Black Filled Polypropylene Homopolymer DescriptionPolyfort® FPP 2121UV-M-31 is a 30% black filled polypropylene homopolymer. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman... |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
ExxonMobil HDPE AA48-002 High Density Polyethylene Resin Product Description: AA48-002 is a blow molding grade high density polyethylene copolymer containing an antistatic additive. It provides a very good balance of stress crack resistance, stiffness and.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
ExxonMobil HDPE HD 6706.62 High Density Polyethylene Copolymer Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
ExxonMobil Paxon™ BA50-100 Blow Molding Resin Product Description: BA50-100 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Availability: .. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
Clariant Renol PPT10 Polypropylene Copolymer, Talc Filled Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
ExxonMobil HD 6706.17 Injection Molding Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM Data |
Dow Retain® PS-4000 Polystyrene Data provided by Dow Chemical. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow UNIVAL™ DMDD-6200 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDD-6200 NT 7 is a multipurpose polymer designed for the high speed production of blow molded containers used to package hous.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow UNIVAL™ DMDF-6200 NT 7 High Density Polyethylene Resin (HDPE) Excellent extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDF-6200 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipme.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
Asahi Kasei Thermofil P-10CC-Y488 10% Calcium Carbonate Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 5 PHR Di-Cup 40C MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |